A liquid phase oxidation of O-xylene with esterification coupling preparation of phthalic acid diester method
The invention relates to a method for preparation of diester phthalate by o-xylene liquid-phase oxidation and esterification coupling. In the presence of a catalyst, air or oxygen is used as an oxygen source for preparation of the diester phthalate by o-xylene liquid-phase oxidation and esterification coupling. The method has the advantages of mild reaction conditions, safe operation, low raw material and energy consumption, high conversion rate and high selectivity and the like.
-