| Properties: | |
| Physical properties of a typical asbestos-reinforced furan polymer are d 1.7, tensile strength 5000 psi, flexural strength 7500 psi, impact strength 0.5 ft lb/in. notch, water absorption 0.2%, and coefficient of thermal expansion 3.0–10−5 in/in/F. | |
| Use: | |
| Coating asphaltic pavements, foundry sand cores, shell molding and corrosion-resistant materials of construction. Since furfural is readily obtainable by heating pentosan-containing products such as corncobs with mineral acid, these resins are inexpensive and have great potential use where products with their characteristics are required. | |