Chemosphere p. 1497 - 1512 (1999)
Update date:2022-08-04
Topics:
Piao, Mingjun
Chu, Shaogang
Zheng, Minghui
Xu, Xiaobai
Polyethylene (PE) was burned in a tube-type furnace with an air flow at a temperature of 600~900°C. Combustion products were collected with glass wool, glass fiber filter, and XAD-2 adsorbent. The analysis of the products was performed with GC-FID and GC-MSD. At low temperature, hydrocarbons were the major components, while at higher temperature the products were composed of polycyclic aromatic hydrocarbons. With the high performance of the Hewlett-Packard 6890GC-5973MSD, more compounds were identified in comparison with previous studies.
View MoreZibo Xiaoguang Chemical Material Co., Ltd
Contact:15954099116
Address:Boshan Development Zone
Shanghai Xinda Pharmaceuticals Co., Ltd.
Contact:86-21-33692333-8008
Address:999 Linxian Road, Jinshan Industrial Park, Shanghai, China
Hangzhou Sartort Biopharma Co., Ltd
website:http://www.sartort.com
Contact:86-571-87039693
Address:No. 57, Tech Park Road, Hangzhou, Zhejiang, China
Jinan Trio PharmaTech Co., Ltd
Contact:86-531-88811783;+(0)13153010282
Address:2766 Yingxiu Road, Jinan High-Tech Zone, China
WENZHOU M&C FOREIGN TRADE CO.,LTD.
Contact:+86-577-88862917
Address:No.8 Liming West Road,Wenzhou,zhejiang,China
Doi:10.1002/adsc.200800801
(2009)Doi:10.1021/om990463h
(1999)Doi:10.1021/jo00833a009
(1970)Doi:10.1016/j.bmcl.2015.12.013
(2016)Doi:10.1021/jo00963a028
(1973)Doi:10.1016/j.materresbull.2014.04.019
(2014)