21 M. Kramer, J.-F. Stumbe, H. Turk, S. Krause, A. Komp,
L. Delineau, S. Prokhorova, H. Kautz and R. Haag, Angew. Chem.,
Int. Ed., 2002, 41, 4252–4256.
hyperbranched copolymers. The copolymers with less branched
shells had higher values of Tm and DHm.
These amphiphilic hyperbranched copolymers could be used
as nanocarriers to efficiently accommodate the hydrophilic
guests, including MO, CR and DB, into the hydrophilic ami-
dated PEI core. The dendritic structure of the shell of these new
nanocarriers contributed pronouncedly to their superior encap-
sulation performance over the nanocarriers with linear shells. As
far as the weight ratio of the encapsulated guests to the nano-
carriers was concerned, the nanocarriers with branched and
linear shells could be tuned to have a similar encapsulation
capacity for the small MO with a mono-sulfonate group.
However, the nanocarriers with branched shells could be
modulated to have a much superior encapsulation capacity to the
nanocarriers with linear shells, for the larger CR and DB with
multi-sulfonate groups.
22 Y. H. Kim and O. W. Webster, J. Am. Chem. Soc., 1990, 112, 4592–
4593.
23 D. Wan, H. Pu and X. Cai, Macromolecules, 2008, 41, 7787–7789.
ꢀ
24 Y. Chen, Z. Shen, L. Pastor-Perez, H. Frey and S.-E. Stiriba,
Macromolecules, 2005, 38, 227–229.
25 H. Liu, Y. Chen, D. Zhu, Z. Shen and S.-E. Stiriba, React. Funct.
Polym., 2007, 67, 383–395.
26 S.-E. Stiriba, H. Kautz and H. Frey, J. Am. Chem. Soc., 2002, 124,
9698–9699.
27 K. R. Kumar and D. E. Brooks, Macromol. Rapid Commun., 2005, 26,
155–159.
28 D. Wan, J. Yuan and H. Pu, Macromolecules, 2009, 42, 1533–1540.
29 D. Wan, G. Wang, H. Pu and M. Jin, Macromolecules, 2009, 42,
6448–6456.
30 J. Zou, Y. Zhao and W. Shi, J. Phys. Chem. B, 2006, 110, 2638–2642.
31 L. Tang, Y. Fang and X. Tang, J. Polym. Sci., Part A: Polym. Chem.,
2005, 43, 2921–2930.
ꢀ
32 Y. Chen, Z. Shen, H. Frey, J. Perez-Prietob and S.-E. Stiriba, Chem.
Commun., 2005, 755–757.
33 R. Haag, Angew. Chem., Int. Ed., 2004, 43, 278–282.
34 Z.-L. Yu, F. Cheng, S.-J. Zhao, J.-W. Zhang, Z.-C. Cai and Y. Chen,
Macromol. Res., 2011, 19, 189–196.
From the experimental results, it can be concluded that for the
effective enhancement of the guest encapsulation performance of
amphiphilic dendritic polymers, besides the well-known methods
of increasing the size and polarity of the core, the introduction of
branching units in the shell is also an effective method.
€
€
35 A. Sunder, M. Kramer, R. Hanselmann, R. Mulhaupt and H. Frey,
Angew. Chem., Int. Ed., 1999, 38, 3552–3555.
36 D. Wan, Y. Lai, M. Jin and H. Pu, Macromol. Chem. Phys., 2011, 212,
1910–1917.
Acknowledgements
37 D. Wan, F. Chen, T. Kakuchi and T. Satoh, Polymer, 2011, 52, 3405–
3412.
38 D. Wan, H. Pu, M. Jin, G. Wang and J. Huang, J. Polym. Sci., Part
A: Polym. Chem., 2011, 49, 2373–2381.
39 D. Wan, H. Pu, M. Jin, H. Pan and Z. Chang, React. Funct. Polym.,
2010, 70, 916–922.
The authors are grateful for the financial support from the
Program for New Century Excellent Talents in University, and
the National Natural Science Foundation of China (20974077,
21074088).
ꢀ
40 M. Calderon, M. A. Quadir, M. Strumia and R. Haag, Biochimie,
2010, 92, 1242–1251.
41 X. Pang, L. Zhao, C. Feng and Z. Lin, Macromolecules, 2011, 44,
7176–7183.
Notes and references
42 M.-C. Jones, M. Ranger and J.-C. Leroux, Bioconjugate Chem., 2003,
14, 774–781.
43 F. Wang, T. K. Bronich, A. V. Kabanov, R. D. Rauh and J. Roovers,
Bioconjugate Chem., 2005, 16, 397–405.
44 H. Liu, Y. Chen, Z. Shen and H. Frey, React. Funct. Polym., 2007, 67,
156–164.
45 Y. Liang, D. Wan, X. Cai, M. Jin and H. Pu, J. Polym. Sci., Part A:
Polym. Chem., 2010, 48, 681–691.
€
1 G. R. Newkome, C. N. Moorefield and F. Vogtle, Dendritic
Molecules: Concepts, Synthesis, Perspectives, VCH, Weinheim, 2001.
2 D. Astruc, E. Boisselier and C. Ornelas, Chem. Rev., 2010, 110, 1857–1959.
3 C. Gao and D. Yan, Prog. Polym. Sci., 2004, 29, 183–275.
4 H. Frauenrath, Prog. Polym. Sci., 2005, 30, 325–384.
5 S. J. Teertstra and M. Gauthier, Prog. Polym. Sci., 2004, 29, 277–327.
6 F. Wurm and H. Frey, Prog. Polym. Sci., 2011, 36, 1–52.
7 D. Wilms, S.-E. Stiriba and H. Frey, Acc. Chem. Res., 2010, 43, 129–
141.
ꢀ
8 K. L. Wooley, C. J. Hawker and J. M. J. Frechet, J. Am. Chem. Soc.,
1993, 115, 11496.
9 Y. Xu, C. Gao, H. Kong, D. Yan, P. Luo, W. Li and Y. Mai,
Macromolecules, 2004, 37, 6264–6267.
10 G. Barrat, Cell. Mol. Life Sci., 2003, 60, 21–37.
11 J. L. Chavez, J. L. Wong, A. V. Jovanovic, E. K. Sinner and
R. S. Duran, IEE Proc.: Nanobiotechnol., 2005, 152, 73–84.
12 M. Irfan and M. Seiler, Ind. Eng. Chem. Res., 2010, 49, 1169–1196.
ꢀ
13 C. J. Hawker, K. L. Wooley and J. M. J. Frechet, J. Chem. Soc.,
Perkin Trans. 1, 1993, 1287–1297.
14 K. R. Copidas, A. R. Leheny, G. Caminati, N. J. Turro and
D. A. Tomalia, J. Am. Chem. Soc., 1991, 113, 1335–1342.
15 S. Stevelmans, J. C. M. van Hest, J. F. G. A. Jansen, D. A. F. J. van
Boxtel, E. M. M. de Brabander-van den Berg and E. W. Meijer,
J. Am. Chem. Soc., 1996, 118, 7398–7399.
46 X. Li, Y. Qian, T. Liu, X. Hu, G. Zhang, Y. You and S. Liu,
Biomaterials, 2011, 32, 6595–6605.
ꢀ
47 S. Hecht and J. M. J. Frechet, Angew. Chem., Int. Ed., 2001, 40, 74–91.
48 P. Furuta and J. M. J. Frechet, J. Am. Chem. Soc., 2003, 125, 13173–
ꢀ
13181.
49 E. Burakowska and R. Haag, Macromolecules, 2009, 42, 5545–5550.
50 S. Xu, Y. Luo and R. Haag, Macromol. Rapid Commun., 2008, 29,
171–174.
51 A. Heise, J. L. Hedrick, C. W. Frank and R. D. Miller, J. Am. Chem.
Soc., 1999, 121, 8647–8648.
52 N. Stavrouli, A. I. Triftaridou, C. S. Patrickios and C. Tsitsilianis,
Macromol. Rapid Commun., 2007, 28, 560–566.
53 F. Wang, T. K. Bronich, A. V. Kabanov, R. D. Rauh and J. Roovers,
Bioconjugate Chem., 2008, 19, 1423–1429.
ꢀ
54 W. Yuan, J. Yuan, S. Zheng and X. Hong, Polymer, 2007, 48, 2585–
2594.
55 X. Cao, Z. Li, X. Song, X. Cui, P. Cao, H. Liu, F. Cheng and
Y. Chen, Eur. Polym. J., 2008, 44, 1060–1070.
16 M. W. P. L. Baars, P. E. Froehling and E. W. Meijer, Chem.
Commun., 1997, 1959–1960.
56 P.-F. Cao, R. Xiang, X.-Y. Liu, C.-X. Zhang, F. Cheng and Y. Chen,
J. Polym. Sci., Part A: Polym. Chem., 2009, 47, 5184–5193.
57 H. Liu, Z. Shen, S.-E. Stiriba, Y. Chen, W. Zhang and L. Wei, J.
Polym. Sci., Part A: Polym. Chem., 2006, 44, 4165–4173.
58 C. Ternat, L. Ouali, H. Sommer, W. Fieber, M. I. Velazco,
17 A. I. Cooper, J. D. Londono, G. Wignall, J. B. McClain,
E. T. Samulski, J. S. Lin, A. Dobrynin, M. Rubinstein,
ꢀ
A. L. C. Burke, J. M. J. Frechet and J. M. DeSimone, Nature,
1997, 389, 368–371.
ꢀ
€
18 A. Garcia-Bernabe, M. Kramer, B. Olah and R. Haag, Chem.–Eur. J.,
ꢁ
C. J. G. Plummer, G. Kreutzer, H.-A. Klok, J.-A. E. Manson and
2004, 10, 2822–2830.
19 A. R. Esker, L.-H. Zhang, C. E. Olsen, K. No and H. Yu, Langmuir,
1999, 15, 1716–1724.
20 R. K. Kainthan and D. E. Brooks, Bioconjugate Chem., 2008, 19,
2231–2238.
A. Herrmann, Macromolecules, 2008, 41, 7079–7089.
59 C. Xia, X. Ding, Y. Sun, H. Liu and Y. Li, J. Polym. Sci., Part A:
Polym. Chem., 2010, 48, 4013–4019.
60 S. Xu, Y. Luo and R. Haag, Macromol. Biosci., 2007, 7, 968–974.
This journal is ª The Royal Society of Chemistry 2012
Soft Matter, 2012, 8, 8361–8369 | 8369