Chemistry Letters p. 2123 - 2126 (1992)
Update date:2022-08-30
Topics:
Mochida, Isao
Aoyagi, Yusuke
Yatsunami, Shunsuke
Fujitsu, Hiroshi
Ethane was found stationally and selectively pyrolyzed into ethylene in first order over a pitch based carbon fiber (CF) by the contract time of 4 second at 948 to 1023 K, which was lower by 200 K than that for the conversional pyrolyses without the fiber.The selectivity tended to decrease moderately with sharp increase of the conversion at higher temperatures, being 97 to 93percent, respectively, at the conversions of 2 and 33percent at 948 and 1023 K, respectively.
View MoreXI'AN CHUKANG BIOTECHNOLOGY CO.,LTD
Contact:29-63685658 63685359
Address:Room 3-1202,Building 1,Oriental oasis,East of Xianning Road,Xi'an,Shaanxi 710043 P.R.China
website:http://www.herbpurify.com
Contact:0086-028-85249238
Address:Room709-C1,Incubator Building, Tianfu Life Science Park No.88,Keyuan Road,Gaoxin district,Chengdu City,Sichuan Prov,China
Golden Union Agrochemical Import and Export Co., Ltd.
Contact:86-755-23910527
Address:Room 1106, Tower 3A, Excellence Century Center, Futian District, Shenzhen, China
Feis International Trade Co,. Ltd
Contact:13961823444-18235944442
Address:Wuxi jiangsu
Daicel Chiral Technologies (China)CO.,LTD
Contact:021-5046-0086*8
Address:Part C, FL 5, the 16th Building, No. 69, XiYa Road, WaiGaoQiao Free Trade Zone, Shanghai, 200131, P.R.China
Doi:10.1021/acs.jced.6b00596
(2017)Doi:10.1021/jo00192a054
(1984)Doi:10.1021/co5001597
(2015)Doi:10.1021/om990977g
(2000)Doi:10.1016/j.tetlet.2004.12.020
(2005)Doi:10.1002/jhet.2753
(2017)