Deposition of thermoelectric strontium hexaboride thin films by a low pressure CVD method
-
Add time:07/29/2019 Source:sciencedirect.com
Thin films of SrB6 were deposited on sapphire substrates using a chemical vapor deposition method, with elemental strontium and decaborane, B10H14, used as the strontium and boron sources, respectively. The formation of highly crystalline, phase-pure SrB6 films was confirmed with X-ray diffraction and reflection high energy diffraction (RHEED) analysis, and the films’ thermoelectric transport properties were measured. A relatively high deposition temperature of 850–950 °C was found to be optimal for obtaining well-crystallized films at an extremely high deposition rate. The thermoelectric transport properties of the SrB6 thin films were observed to be comparable to those reported for bulk materials, but an unexpectedly high electrical resistivity led to a reduced power factor value for the thin films.
We also recommend Trading Suppliers and Manufacturers of STRONTIUM BORIDE (cas 12046-54-7). Pls Click Website Link as below: cas 12046-54-7 suppliers
Prev:Preparation of a series of lanthanide borohydrides and their thermal decomposition to refractory lanthanide borides
Next:A comparative study of strontium and titanium doped mullite in PVDF matrix and their phase behavior, microstructure and electrical properties) - 【Back】【Close 】【Print】【Add to favorite 】
- Related Information
- Evaluations of antimony and strontium interaction in an Al–Si–Cu–Zn die cast alloy08/01/2019
- Classification of borides07/31/2019
- A comparative study of strontium and titanium doped mullite in PVDF matrix and their phase behavior, microstructure and electrical properties07/30/2019
- Preparation of a series of lanthanide borohydrides and their thermal decomposition to refractory lanthanide borides07/28/2019
- Mechanically induced combustion synthesis and thermoelectric properties of nanostructured strontium hexaboride (SrB6)07/27/2019
-
Health and Chemical more >