The use of pyrrhotite-containing aggregate in concrete has led to the premature deterioration of building foundations in Connecticut (U.S.A.). Pyrrhotite is a highly reactive iron-sulfide mineral that can initiate internal sulfate attack in concrete structures, because it serves as a source of sulfate ions for secondary minerals. Associated increases in mineral volume can lead to spalling, cracking and a loss of structural integrity. Since pyrrhotite is a strongly ferrimagnetic mineral with a Curie-temperature of 325 °C and several diagnostic phase transitions, we measured the variation of magnetic susceptibility between room-temperature and 700 °C. Such a thermomagnetic measurement serves as a rapid and sensitive semi-quantitative indicator of pyrrhotite in aggregate or concrete samples. In combination with measurements of total sulfur concentrations, pyrrhotite concentrations as low as 0.1% can be detected. The analysis can aid in the quantification of risk of internal sulfur attack due to the presence of pyrrhotite.
We also recommend Trading Suppliers and Manufacturers of PYRRHOTITE (cas 12305-96-3). Pls Click Website Link as below: cas 12305-96-3 suppliers
Prev:Flotation recovery–by–size comparison of PYRRHOTITE (cas 12305-96-3) superstructures with and without depressants
Next:Water quality effects on bubble-particle attachment of PYRRHOTITE (cas 12305-96-3)) - 【Back】【Close 】【Print】【Add to favorite 】
- Related Information
- Deterioration of residential concrete foundations: The role of PYRRHOTITE (cas 12305-96-3)-bearing aggregate08/16/2019
- Nutrient removal through PYRRHOTITE (cas 12305-96-3) autotrophic denitrification: Implications for eutrophication control08/15/2019
- The role of Cu ion activation and surface oxidation for polymorphic PYRRHOTITE (cas 12305-96-3) flotation performance in Strathcona Mill08/14/2019
- 57Fe NMR characterisation of PYRRHOTITE (cas 12305-96-3)08/13/2019
- Effect of acidic activators on the flotation of oxidized PYRRHOTITE (cas 12305-96-3)08/12/2019
- Water quality effects on bubble-particle attachment of PYRRHOTITE (cas 12305-96-3)08/11/2019
- Flotation recovery–by–size comparison of PYRRHOTITE (cas 12305-96-3) superstructures with and without depressants08/09/2019