  • Thermal conductivity modification of n-Octanoic acid (cas 124-07-2)-myristic acid composite phase change material

  • Add time:09/26/2019    Source:sciencedirect.com

    Considering the low thermal conductivity of organic phase change materials (PCMs), a modification of Octanoic acid (OA) and Myristic acid (MA) binary mixture with a mass ratio of 87:13 was studied. The influence of expanded graphite (EG) and Hydroxylated multi-walled carbon nanotubes (MWCNTs) on the thermal conductivity of OA-MA were compared and analyzed. The morphology of these two nanoparticals and OA-MA/EG PCM were measured by scanning electronic microscope (SEM). 7 wt% EG was finally selected as the additive to modify the thermal conductivity of OA-MA. By differential scanning calorimeter (DSC), the phase transition temperature was measured to be 6.8 °C and the enthalpy of fusion was 136.3 J/g. The thermal conductivity of OA-MA/EG was 0.9975 W/(m·K) tested by Hot Disk, which remarkably increased by 235.75% compared with the thermal conductivity of OA-MA. Undergoing 100 freeze-thaw cycles, the properties of the OA-MA/EG did not change significantly, which shows the composite PCM is especially suitable for its application in pharmaceutical refrigerated transport system.

    We also recommend Trading Suppliers and Manufacturers of Octanoic acid (cas 124-07-2). Pls Click Website Link as below: cas 124-07-2 suppliers

    Prev:Deoxygenation of Octanoic acid (cas 124-07-2) catalyzed by hollow spherical Ni/ZrO2
    Next:Differences in crystal growth behaviors of boehmite particles with Octanoic acid (cas 124-07-2) and sodium octanoate under supercritical hydrothermal conditions)

  • Back】【Close 】【Print】【Add to favorite
Periodic Table
    Related Products