Chemistry Letters p. 751 - 752 (1998)
Update date:2022-08-11
Topics:
Ohno, Hiroyuki
Ito, Kaori
Vinyl polymers having either imidazolium group or sulfonamide group in the side chain were prepared as components to form a molten salt. After mixing, these polymers formed a molten-salt-like flexible domain in the polymer, and excellent ionic conductivity (7.52 X 10-6 Scm-1 and 1.88 X 10-4 Scm-1 at 30°C, respectively) was observed in spite of their rubber-or powder-like properties.
View MoreBaoding City Light Industry And Textiles Imp.& Exp. Corp. Chemical Department.
Contact:86-312-3262436
Address:NO.658 CHAOYANG SOUTH STREET,BAODING CITY HEBEI CHINA
Weihao Chemtech (ChangZhou) Co., Ltd.(expird)
Contact:051989185693
Address:NO 217 huangshan Rd ,Changzhou
Lanzhou huibang biological chemical technology Co., LTD
Contact:0931-7843964
Address:NO.2011,Yannan Road,Chengguan,
Ji'an Kexin Trade Co., Ltd.(expird)
Contact:86-0796-8187704 18507063190
Address:ji'an jiangxi
Chengdu Chengnuo New-Tech Co., Ltd
Contact:0086-028-85749078
Address:4 Jiuyang road,Jiulong industrial port,Chengdu, China
Doi:10.1007/s11164-014-1634-5
(2015)Doi:10.1246/bcsj.61.1281
(1988)Doi:10.1021/ja01133a033
(1952)Doi:10.1007/s11164-017-3235-6
(2018)Doi:10.1006/jcat.1999.2418
(1999)Doi:10.1055/s-1975-23933
(1975)