Journal of Materials Science p. 420 - 424 (1989)
Update date:2022-08-24
Topics:
Itoh
Matsudaira
Naka
Hamamoto
TiB2 powder was synthesized by a controlled formation reaction from titanium metal and amorphous boron. Precursory TiB2 formed by the pretreatment of the mixed powder (mole ratio: B/Ti = 2.0) at 600°C for 60 min in an argon stream. H
View MoreJiangsu Zhenfang Chemical CO.,LTD.(Suzhou Zhenfang Chemical Factory)
Contact:+86-512-69598882
Address:Room1201, Jiayuan Road No.1018, Xiangcheng District, Suzhou, China
LianYunGang Chiral Chemical(CHINA) CO.,LTD
Contact:+86-518-83616958 +86-519-82884848
Address:LianYunGang Chemical Industry Park (JiangSu)
Hunan Dinuo Pharmaceutical Co.,Ltd.
Contact:86-731-88280100*8561
Address:Bio-pharmaceutical industrial park, Liuyang, Hunan, China
Beyond Pharmaceutical Co., Ltd
Contact:+86-571-8195-3185
Address:No. 13-1, Liansheng Road, Yuhang District
website:http://www.arromax.com
Contact:+86-0512-62959601 skype:aimmezhang
Address:Suite 401, Bldg A3, 218 Xinghu St.Suzhou Industrial Park 215123, P.R. China
Doi:10.1039/P29900001991
(1990)Doi:10.1002/jps.2600821214
(1993)Doi:10.1039/c7cc02105d
(2017)Doi:10.1016/j.saa.2019.117867
(2020)Doi:10.1021/jacs.5b01435
(2015)Doi:10.1016/j.tet.2019.05.039
(2019)