Journal of Solid State Chemistry p. 47 - 51 (1988)
Update date:2022-08-16
Topics:
Davison
Kershaw
Dwight
Wold
Samples of cubic ZrO//2 containing 2. 5-40 at% Fe(III) were prepared by codecomposition of the nitrates, X-ray powder diffraction analysis and magnetic measurements indicated that alpha -Fe//2O//3 and ZrO//2 form a solid solution up to 25 at% Fe/Zr in the product. At this point, the solubility limit of a-Fe//2O//3 in ZrO//2 is exceeded. The reduction of cubic zirconia samples containing 2. 5-20 at% Fe(III) leads to the stabilization of iron(II) in the zirconia lattice. Reduction to metallic iron occurs at much higher temperatures than the reduction of bulk a-Fe//2O//3.
Wuxi Pharma-Trading Import & Export Co.,Ltd.
Contact:+86-510-82304590 82716390
Address:Room 523,Youzu Alliance Building,No.88 Renmin Zhonglu,Wuxi,Jiangsu,China
Shanghai Minstar Chemical Co., Ltd
website:http://www.minstargroup.com
Contact:86-21-18019205509
Address:BUILDING 8, NO.1098, CHUANSHA ROAD, SHANGHAI, CHINA
Guangxi Shanyun Biochemical Science and Technology Co., Ltd
Contact:+86-0772--6828887
Address:#2 Industrial Park of Luzhai County, Liuzhou, Guangxi, China
Synochem Ingredients Corp., Ltd.
Contact:+86-512-5636 2180
Address:Zhangjiagang Free Trade Zone
Contact:+86-571-86025531 / 86024803
Address:1218-24 Guangyin Mansion,42 Fengqi East Road
Doi:10.1016/S0020-1693(00)87278-3
(1978)Doi:10.1016/j.molstruc.2017.02.079
(2017)Doi:10.1016/S0022-328X(00)85739-3
(1979)Doi:10.1007/BF01417974
(1981)Doi:10.1016/j.tet.2021.132413
(2021)Doi:10.1021/jo00101a024
(1994)