LiAlO2 was prepared by two sol-gel methods using simultaneous hydrolysis of the reagents: aluminum sec-butoxide/ lithium methoxide and aluminum sec-butoxide/LiOH. The resulting ceramic powders were compared with those prepared by two conventional methods (i.e., solid-state fusion and peroxide). The sol-gel method provided powders with a very high γ-LiAlO2 content after calcining at temperatures as low as 700°C when LiOH was used. The solids were characterized by AAS, DTA, TGA, XRD, and SEM.
website:https://www.synose.com/
Contact:86-579-82275537
Address:No.1958 Liyu Road , jinhua,zhejiang,China
Changsha Huajing Powdery Material Technological Co., Ltd.
Contact:86-731-88879686
Address:Building 2, West Garden, Main Campus of Central South University, Changsha, Hunan Province, China
Shenzhen HwaGen Pharmaceutical Co., Ltd
website:http://www.rafflespt.com
Contact:+86-752-5538396
Address:Guangdong Huizhou China
ShanDong XinDa Chemical CO.,LTD(expird)
Contact:086-0311-87580543
Address:No.168, High Technology Development Zone Jinan Shandong China
Jiangxi Huashi Pharmaceutical Co., Ltd
Contact:+86-795-4509628
Address:Ningbo Ave., Fengtian Industrial Park, Fengxin Country, Jiangxi, China.
Doi:10.1021/ja01642a025
(1954)Doi:10.1021/jo01078a602
(1960)Doi:10.1021/acs.orglett.6b02649
(2016)Doi:10.1007/s10562-016-1759-9
(2016)Doi:10.1016/0040-4039(95)01278-P
(1995)Doi:10.1016/j.jphotochem.2018.07.043
(2018)